聚碳酸酯(PC) by Mando Advanced Materials Co., Ltd.
产品 | 可用性 | 产品说明 |
---|---|---|
TEKALOY™ G70A2 | 亚太地区 |
Features
- G70A2 is a PC/ABS alloy unreinforced product.
Application
- E/E parts.
Drying
- Product is dried and packed with a moisture content of <0.16%. Should the Packaging become damaged or be left open too long, then the material must be Dried. A too high moisture content can lead to a reduction of optical and Mechanical properties.
|
TEKALOY™ G70A3 | 亚太地区 |
Features
- G70A3 is a PC/ABS alloy unreinforced with heat resistance.
Application
- E/E parts.
Drying
- Product is dried and packed with a moisture content of <0.16%. Should the Packaging become damaged or be left open too long, then the material must be Dried. A too high moisture content can lead to a reduction of optical and Mechanical properties.
|
TEKALOY™ G70A4 | 亚太地区 |
Features
- TEKALOY G70A4 is unreinforced PC/ABS alloy.
Application
- Miscellaneous Goods
Drying
- Product is dried and packed with a moisture content of <0.16%. Should the Packaging become damaged or be left open too long, then the material must be Dried. A too high moisture content can lead to a reduction of optical and Mechanical properties.
|
TEKALOY™ G70NH | 亚太地区 |
Features
- G70NH is a non halogen flame retardant PC/ABS .
Application
- IT&OA
Drying
- Product is dried and packed with a moisture content of <0.16%. Should the Packaging become damaged or be left open too long, then the material must be Dried. A too high moisture content can lead to a reduction of optical and Mechanical properties.
|
TEKALOY™ G70NHT | 亚太地区 |
Features
- G70NHT is a PC/ABS alloy. G70NHT has good properties with high flow, impact resistance, flame retardant and good processability.
Application
- Automotive & E/E parts.
Drying
- Product is dried and packed with a moisture content of <0.16%. Should the Packaging become damaged or be left open too long, then the material must be Dried. A too high moisture content can lead to a reduction of optical and Mechanical properties.
|
TEKALOY™ G75NHT | 亚太地区 |
Features
- TEKALOY G75NHT is a brominated flame retardant PC/ABS .
Application
- Elecric and Electronic Housing and Components
Drying
- Product is dried and packed with a moisture content of <0.16%. Should the Packaging become damaged or be left open too long, then the material must be Dried. A too high moisture content can lead to a reduction of optical and Mechanical properties.
|
TEKANATE™ G7007 | 亚太地区 |
Features
- G7007 is a unreinforced polycarbonate with MFI 6g/10min.
Application
- Electric & Electronic (Housing, Components)
Drying
- Product is dried and packed with a moisture content of <0.16%. Should the Packaging become damaged or be left open too long, then the material must be Dried. A too high moisture content can lead to a reduction of optical and Mechanical properties.
|
TEKANATE™ G7010 | 亚太地区 |
Features
- G7010 is a unreinforced polycarbonate with MFI 10g/10min.
Application
- E&E Housing and Components, Automotive Exterior and Interior
Drying
- Product is dried and packed with a moisture content of <0.16%. Should the Packaging become damaged or be left open too long, then the material must be Dried. A too high moisture content can lead to a reduction of optical and Mechanical properties.
|
TEKANATE™ G7010FR | 亚太地区 |
Features
- G7010FR is a unreinforced polycarbonate with MFI 10g/10min. G7010FR has good properties with flammability UL94 V-0 and good processability.
Application
- Electric & Electronic Housing and Components.
Drying
- Product is dried and packed with a moisture content of <0.16%. Should the Packaging become damaged or be left open too long, then the material must be Dried. A too high moisture content can lead to a reduction of optical and Mechanical properties.
|
TEKANATE™ G7013 | 亚太地区 |
Features
- G7013 is a unreinforced polycarbonate with MFI 13g/10min.
Application
- E&E Housing and Components Automotive Exterior and Interior.
Drying
- Product is dried and packed with a moisture content of <0.16%. Should the Packaging become damaged or be left open too long, then the material must be Dried. A too high moisture content can lead to a reduction of optical and Mechanical properties.
|
TEKANATE™ G7013FR | 亚太地区 |
Features
- G7013FR is a unreinforced polycarbonate with MFI 13g/10min. G7013FR has good properties with flammability UL94 V-0 and good processability.
Application
- Electric & Electronic Housing and Components.
Drying
- Product is dried and packed with a moisture content of <0.16%. Should the Packaging become damaged or be left open too long, then the material must be Dried. A too high moisture content can lead to a reduction of optical and Mechanical properties.
|
TEKANATE™ G7020 | 亚太地区 |
Features
- G7020 is a unreinforced polycarbonate with MFI 20g/10min.
Application
- E&E Housing and Components Automotive Interior.
Drying
- Product is dried and packed with a moisture content of <0.16%. Should the Packaging become damaged or be left open too long, then the material must be Dried. A too high moisture content can lead to a reduction of optical and Mechanical properties.
|
TEKANATE™ G7038 | 亚太地区 |
Features
- G7038 is a unreinforced polycarbonate with MFI 38g/10min.
Application
- E&E Housing and Components Automotive Interior.
Drying
- Product is dried and packed with a moisture content of <0.16%. Should the Packaging become damaged or be left open too long, then the material must be Dried. A too high moisture content can lead to a reduction of optical and Mechanical properties.
|
TEKANATE™ G710 | 亚太地区 |
Features
- G710 is GF 10% reinforced Polycarbonate. G710 has good properties with good mechanical properties.
Application
- E&E Housing and Components Automotive. (Interior)
Drying
- Product is dried and packed with a moisture content of <0.16%. Should the Packaging become damaged or be left open too long, then the material must be Dried. A too high moisture content can lead to a reduction of optical and Mechanical properties.
|
TEKANATE™ G720 | 亚太地区 |
Features
- G720 is GF 20% reinforced Polycarbonate. G720 has good properties with good mechanical properties.
Application
- E&E Housing and Components Automotive. (Interior)
Drying
- Product is dried and packed with a moisture content of <0.16%. Should the Packaging become damaged or be left open too long, then the material must be Dried. A too high moisture content can lead to a reduction of optical and Mechanical properties.
|