Polyphenylene Sulfide (PPS): TEDUR®
Produto | Disponibilidade | Descrição do produto |
---|---|---|
TEDUR® L 9105-1 | América do Norte |
Base Polymer
Polyphenylene Sulphide
Filler/Additive System
30 % glass fibres
Special Features
high toughness, high stiffness
Market Segment
Automotive, Machinery
Application Area
injection moulded parts
|
TEDUR® L 9107-1 S | América do Norte |
Base Polymer
Polyphenylene Sulphide
Filler/Additive System
40 % glass fibres
Special Features
injection moulding, high toughness, reduced flash, increased burst strength
Market Segment
Machinery
Application Area
pump components
Typical Applications
pump impellers
|
TEDUR® L 9107-1 U | América do Norte |
Base Polymer
Polyphenylene Sulphide
Filler/Additive System
40 % glass fibres
Special Features
injection moulding grade, high toughness, reduced flash, increased burst strength
Application Area
pump components
Typical Applications
pump impellers
|
TEDUR® L 9107-1 | América do Norte |
Base Polymer
Polyphenylene Sulphide
Filler/Additive System
40 % glass fibres
Special Features
injection moulding grade, high toughness, reduced flash, increased burst strength
Application Area
pump components
Typical Applications
pump impellers
|
TEDUR® L 9107-7 | América do Norte |
Base Polymer
Polyphenylene Sulphide
Filler/Additive System
40 % glass fibres
Special Features
injection moulding grade, high toughness, reduced flash, increased burst strength, low odour
Market Segment
Automotive, Machinery, various
Application Area
pump components
Typical Applications
housings, pump impellers, high pressure vessels
|
TEDUR® L 9113-2 | América do Norte |
Base Polymer
Polyphenylene Sulphide
Filler/Additive System
60 % glass fibres
Special Features
high stiffness
Market Segment
Automotive, Machinery
Application Area
injection moulding grade
|
TEDUR® L 9114-1 S | América do Norte |
Base Polymer
Polyphenylene Sulphide
Filler/Additive System
60 % glass fibres
Special Features
high stiffness, injection moulding grade
Typical Applications
various
|
TEDUR® L 9116-1 | América do Norte |
Base Polymer
Polyphenylene Sulphide
Filler/Additive System
60 % glass fibres
Special Features
low warpage, high toughness, high stiffness
Market Segment
Automotive, Machinery
Application Area
injection moulded parts
|
TEDUR® L 9200-1 U | América do Norte |
Base Polymer
Polyphenylene Sulphide
Filler/Additive System
60 % glass fibre/mineral
Special Features
high toughness, high stiffness, low warpage, low anisotropic shrinkage
Market Segment
Automotive, various
Typical Applications
seals, various
|
TEDUR® L 9200-1 | América do Norte |
Base Polymer
Polyphenylene Sulphide
Filler/Additive System
60 % glass fibre/mineral
Special Features
high toughness
Market Segment
Automotive, various
Typical Applications
seals, various
|
TEDUR® L 9214-1 | América do Norte |
Base Polymer
Polyphenylene Sulphide
Filler/Additive System
45 % glass fibres, 20 % mineral
Special Features
high stiffness
Market Segment
Automotive, Machinery
Typical Applications
highly stressed parts
|
TEDUR® L 9217-1 S | América do Norte |
Base Polymer
Polyphenylene Sulphide
Filler/Additive System
65 % glass fibre/mineral
Special Features
high stiffness, hot oil resistant, good hydrolysis resistant
Market Segment
Automotive, Machinery, Lighting
Typical Applications
highly stressed parts
|
TEDUR® L 9217-1 | América do Norte |
Base Polymer
Polyphenylene Sulphide
Filler/Additive System
65 % glass fibre/mineral
Special Features
high stiffness, hot oil resistant, good hydrolysis resistant
Market Segment
Automotive, Machinery, Lighting
Typical Applications
highly stressed parts
|
TEDUR® L 9220-1 | América do Norte |
Base Polymer
Polyphenylene Sulphide
Filler/Additive System
65 % glass fibre/mineral
Special Features
high stiffness, good hydrolysis resistant, oil resistant
Market Segment
Automotive, Machinery
Application Area
injection moulded parts
Typical Applications
highly stressed parts
|
TEDUR® L 9300-1 | América do Norte |
Base Polymer
Polyphenylene Sulphide
Filler/Additive System
40 % glass fibres / glass beads
Colour
black
Special Features
high toughness, reduced flash, increased burst strength, low warpage
Typical Applications
various
|
TEDUR® L 9310-4 S | América do Norte |
Base Polymer
Polyphenylene Sulphide
Filler/Additive System
mineral, glass beads
Special Features
improved surface, metallizable
Typical Applications
various
|
TEDUR® L 9400-1 | América do Norte |
Base Polymer
Polyphenylene Sulphide
Filler/Additive System
15 % carbon fibres
Special Features
reduced surface resistivity, electrically conductive, high stiffness
Market Segment
Automotive, Machinery, electrical and electronic
Typical Applications
functional components
|
TEDUR® L 9400-3.2 | América do Norte |
Base Polymer
Polyphenylene Sulphide
Filler/Additive System
15 % carbon fibres
Special Features
reduced surface resistivity, electrically conductive, high stiffness
Market Segment
Automotive, Machinery, electrical and electronic
Typical Applications
functional components
|
TEDUR® L 9401-1 | América do Norte |
Base Polymer
Polyphenylene Sulphide
Filler/Additive System
40 % glass fibres, 5 % PTFE
Special Features
improved sliding / wear, high stiffness
Market Segment
Automotive, Machinery
Typical Applications
bearings and sliding elements, functional components
|
TEDUR® L 9404-3.2 | América do Norte |
Base Polymer
Polyphenylene Sulphide
Filler/Additive System
30 % carbon fibres
Special Features
reduced surface resistivity, electrically conductive, high stiffness
Market Segment
Automotive, Machinery, electrical and electronic
Typical Applications
functional components
|
TEDUR® L 9406-1 | América do Norte |
Base Polymer
Polyphenylene Sulphide
Filler/Additive System
10 % carbon fibres, 50 % glass fibre/mineral
Special Features
electrically conductive, high stiffness, low warpage
Market Segment
Automotive, Machinery
Application Area
injection moulded parts
Typical Applications
bearings and sliding elements, functional components
|
TEDUR® L 9409-3.2 | América do Norte |
Base Polymer
Polyphenylene Sulphide
Filler/Additive System
30 % carbon fibres, 15 % PTFE
Special Features
reduced surface resistivity, electrically conductive, improved sliding / wear
Market Segment
Automotive, Machinery, electrical and electronic
Typical Applications
functional components, housings, bearings and sliding elements
|
TEDUR® L 9410-1 | América do Norte |
Base Polymer
Polyphenylene Sulphide
Filler/Additive System
45 % glass fibre/mineral, 15 % PTFE
Special Features
improved sliding / wear, high stiffness, low warpage
Market Segment
Automotive, Machinery
Typical Applications
bearings and sliding elements, functional components
|
TEDUR® L 9412-3.2 | América do Norte |
Base Polymer
Polyphenylene Sulphide
Filler/Additive System
10 % carbon fibres, 10 % graphite, 10 % PTFE
Special Features
reduced surface resistivity, electrically conductive, improved sliding / wear
Market Segment
Automotive, Machinery, electrical and electronic
Typical Applications
functional components, housings, bearings and sliding elements
|
TEDUR® L 9413-1 | América do Norte |
Base Polymer
Polyphenylene Sulphide
Filler/Additive System
15 % carbon fibres, 15 % PTFE, 4 % silicone
Special Features
improved sliding / wear, high stiffness, electrically conductive, scratch resistant
Market Segment
Automotive, Machinery
Typical Applications
bearings and sliding elements, functional components
|
TEDUR® L 9421-1 S | América do Norte |
Base Polymer
Polyphenylene Sulphide
Filler/Additive System
40 % glass fibres, 10 % PTFE
Special Features
improved sliding / wear, high stiffness, high toughness
Market Segment
Automotive, Machinery
Typical Applications
bearings and sliding elements, functional components
|
TEDUR® L 9422-1 | América do Norte |
Base Polymer
Polyphenylene Sulphide
Filler/Additive System
30 % glass fibres, 15 % PTFE
Special Features
improved sliding / wear, high stiffness, high toughness
Market Segment
Automotive, Machinery
Typical Applications
bearings and sliding elements, functional components
|
TEDUR® L 9510-1 S | América do Norte |
Base Polymer
Polyphenylene Sulphide
Filler/Additive System
40 % glass fibres
Special Features
injection moulding, high stiffness
Market Segment
Machinery
Application Area
pump components
Typical Applications
various
|
TEDUR® L 9510-1 | América do Norte |
Base Polymer
Polyphenylene Sulphide
Filler/Additive System
40 % glass fibres
Special Features
high stiffness
Application Area
pump components
Typical Applications
various
|
TEDUR® L 9510-5 | América do Norte |
Base Polymer
Polyphenylene Sulphide
Filler/Additive System
40 % glass fibres
Special Features
injection moulding grade, high stiffness, easy flow
Market Segment
various
Application Area
pump components
Typical Applications
housings
|
TEDUR® L 9511 | América do Norte |
Base Polymer
Polyphenylene Sulphide
Filler/Additive System
45 % glass fibres
Special Features
high stiffness
Application Area
various
Typical Applications
housings, fixing elements
|
TEDUR® L 9511-2 | América do Norte |
Base Polymer
Polyphenylene Sulphide
Filler/Additive System
45 % glass fibres
Special Features
high stiffness
Market Segment
Automotive, Machinery
Application Area
injection moulded parts
Typical Applications
pump components, pump impellers, housings, high pressure vessels
|
TEDUR® L 9523 | América do Norte |
Base Polymer
Polyphenylene Sulphide
Filler/Additive System
60 % glass fibre/mineral
Colour
black
Special Features
high stiffness, improved surface appearance
Application Area
various
Typical Applications
reflectors, various
|
TEDUR® L 9560 S | América do Norte |
Base Polymer
Polyphenylene Sulphide
Filler/Additive System
50 % mineral
Special Features
improved surface appearance, high surface gloss, metallizable
Application Area
injection moulding grade
Typical Applications
reflectors
|
TEDUR® L 9560 | América do Norte |
Base Polymer
Polyphenylene Sulphide
Filler/Additive System
50 % mineral
Special Features
improved surface appearance, high surface gloss
Market Segment
Automotive, Machinery
Application Area
injection moulded parts
Typical Applications
reflectors
|
TEDUR® L 9903-1 | América do Norte |
Base Polymer
Polyphenylene Sulphide
Filler/Additive System
70 % special filler
Special Features
increased thermal conductivity, electrostatically dissipating, high density, magnetisable
Market Segment
Automotive, Machinery, electrical and electronic
Application Area
electrical components
Typical Applications
coil formers / bobbins
|
TEDUR® L 9904-1 | América do Norte |
Base Polymer
Polyphenylene Sulphide
Filler/Additive System
80 % special filler
Special Features
increased thermal conductivity, electrostatically dissipating, high density, magnetisable
Market Segment
Automotive, Machinery, electrical and electronic
Application Area
electrical components
Typical Applications
coil formers / bobbins
|
TEDUR® L 9912-1 | América do Norte |
Base Polymer
Polyphenylene Sulphide
Filler/Additive System
60 % glass fibre/mineral
Special Features
high density
Market Segment
Automotive, Machinery
Application Area
injection moulded parts
Typical Applications
various
|
TEDUR® L FC 9510-5 | América do Norte |
Base Polymer
Polyphenylene Sulphide
Filler/Additive System
40 % glass fibres
Special Features
high stiffness, easy flow
Market Segment
Machinery, electrical and electronic, building and construction
Application Area
injection moulded parts, pump components
Typical Applications
housings, Parts in contact with drinking water
|
TEDUR® L FC 9510-6 | América do Norte |
Base Polymer
Polyphenylene Sulphide
Filler/Additive System
40 % glass fibres
Special Features
high stiffness
Market Segment
Machinery
Application Area
pump components, ducting / piping systems
Typical Applications
pipe fitting
|