Polybutadiene Rubber (PBR): HIPREN®
製品 | 可用性 | 製品の説明 |
---|---|---|
HIPREN® EM 1500 T | アジア太平洋地域 |
HIPREN® EM 1500 T is produced by cold copolymerisation process, with the use of rosin acids soaps as emulsifiers, and contains 23.5% styrene bounded in polymer. The rubber is stabilised with staining antioxidant added during the production process.
HIPREN® EM 1500T is dark coloured, without nitrosoamine.
HIPREN® EM 1500 T is compatible with natural rubber and other synthetic rubbers. Good compatibility, easy incorporation of various compounding ingredients provide possibility of mixing formulations for different applications requirement.
Application:
HIPREN EM 1500 T is used for production of wide range products including simple small articles, moulded and pressed products, light pneumatics and heavy conveyer belts, hoses, tires etc.
|
HIPREN® EM 1502 T | アジア太平洋地域 |
HIPREN® EM 1502 T is produced by cold copolymerisation process, with the use of rosin and fatty acids soaps as emulsifiers, and contains 23.5% styrene bounded in polymer. The rubber is stabilised with non-staining antioxidant. HIPREN® EM 1502 T is light coloured, without nitrosoamine.
HIPREN® EM 1502 T is compatible with natural rubber and other synthetic rubbers. Good compatibility, easy incorporation of various compounding ingredients provide possibility of mixing formulations for different applications requirement.
Application:
HIPREN EM 1502 T is used for production of light coloured compounds and products requiring high transparency including light coloured wheel sides, sport goods, flooring, medical and house hold articles.
HIPREN® EM 1502 T has Health Certificate issued by Institute for Health Protection of Serbia
|
HIPREN® EM 1712 T TDAE | アジア太平洋地域 |
HIPREN® EM 1712 T TDAE (HIPREN EM 1723) contains 23.5% styrene bounded in polymer. It is extended with 37.5 parts (w/w) of low aromatic TDAE oil per 100.0 parts (w/w) of polymer. The rubber is produced by low temperature emulsion copolymerization process with the use of resin and fatty acids soaps as emulsifiers and is coagulated by acid. The rubber contains a staining stabiliser added during the production process. The product is without nitrosoamine.
|