Polykarbonat (PC): TEKANATE™
Produkt | Verfügbarkeit | Produktbeschreibung |
---|---|---|
TEKANATE™ G7007 | Asien Pazifik |
Features
- G7007 is a unreinforced polycarbonate with MFI 6g/10min.
Application
- Electric & Electronic (Housing, Components)
Drying
- Product is dried and packed with a moisture content of <0.16%. Should the Packaging become damaged or be left open too long, then the material must be Dried. A too high moisture content can lead to a reduction of optical and Mechanical properties.
|
TEKANATE™ G7010 | Asien Pazifik |
Features
- G7010 is a unreinforced polycarbonate with MFI 10g/10min.
Application
- E&E Housing and Components, Automotive Exterior and Interior
Drying
- Product is dried and packed with a moisture content of <0.16%. Should the Packaging become damaged or be left open too long, then the material must be Dried. A too high moisture content can lead to a reduction of optical and Mechanical properties.
|
TEKANATE™ G7010FR | Asien Pazifik |
Features
- G7010FR is a unreinforced polycarbonate with MFI 10g/10min. G7010FR has good properties with flammability UL94 V-0 and good processability.
Application
- Electric & Electronic Housing and Components.
Drying
- Product is dried and packed with a moisture content of <0.16%. Should the Packaging become damaged or be left open too long, then the material must be Dried. A too high moisture content can lead to a reduction of optical and Mechanical properties.
|
TEKANATE™ G7013 | Asien Pazifik |
Features
- G7013 is a unreinforced polycarbonate with MFI 13g/10min.
Application
- E&E Housing and Components Automotive Exterior and Interior.
Drying
- Product is dried and packed with a moisture content of <0.16%. Should the Packaging become damaged or be left open too long, then the material must be Dried. A too high moisture content can lead to a reduction of optical and Mechanical properties.
|
TEKANATE™ G7013FR | Asien Pazifik |
Features
- G7013FR is a unreinforced polycarbonate with MFI 13g/10min. G7013FR has good properties with flammability UL94 V-0 and good processability.
Application
- Electric & Electronic Housing and Components.
Drying
- Product is dried and packed with a moisture content of <0.16%. Should the Packaging become damaged or be left open too long, then the material must be Dried. A too high moisture content can lead to a reduction of optical and Mechanical properties.
|
TEKANATE™ G7020 | Asien Pazifik |
Features
- G7020 is a unreinforced polycarbonate with MFI 20g/10min.
Application
- E&E Housing and Components Automotive Interior.
Drying
- Product is dried and packed with a moisture content of <0.16%. Should the Packaging become damaged or be left open too long, then the material must be Dried. A too high moisture content can lead to a reduction of optical and Mechanical properties.
|
TEKANATE™ G7038 | Asien Pazifik |
Features
- G7038 is a unreinforced polycarbonate with MFI 38g/10min.
Application
- E&E Housing and Components Automotive Interior.
Drying
- Product is dried and packed with a moisture content of <0.16%. Should the Packaging become damaged or be left open too long, then the material must be Dried. A too high moisture content can lead to a reduction of optical and Mechanical properties.
|
TEKANATE™ G710 | Asien Pazifik |
Features
- G710 is GF 10% reinforced Polycarbonate. G710 has good properties with good mechanical properties.
Application
- E&E Housing and Components Automotive. (Interior)
Drying
- Product is dried and packed with a moisture content of <0.16%. Should the Packaging become damaged or be left open too long, then the material must be Dried. A too high moisture content can lead to a reduction of optical and Mechanical properties.
|
TEKANATE™ G720 | Asien Pazifik |
Features
- G720 is GF 20% reinforced Polycarbonate. G720 has good properties with good mechanical properties.
Application
- E&E Housing and Components Automotive. (Interior)
Drying
- Product is dried and packed with a moisture content of <0.16%. Should the Packaging become damaged or be left open too long, then the material must be Dried. A too high moisture content can lead to a reduction of optical and Mechanical properties.
|